| 对应标准 |
SAE AMS 5662N-2016
自耗电极或真空感应熔炼 1775°F (968°C) 、固溶热处理和脱溶淬硬 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50AI - 18Fe 耐腐蚀和耐热镍合金棒材、锻件和环件 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50AI - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable |